After bending a stainless steel enclosure, the bend angles and dimensions may meet the specs. 그렇지만, two die shoulder marks are formed on the surface. These marks are usually removed by polishing, thereby increasing the total cost of the job. It is more difficult to achieve the original surface finish of a brushed stainless steel or coated sheet metal. In these instances, the contact of the lower die to the sheet metal determines the surface quality of the finished part.
A non-marking press brake die improves surface quality of fabricated parts by changing the contact material or the way the sheet metal is supported during bending. An adjustable V-opening roller die in conjunction with rolling contact and a variable V-opening, makes it ideal for fabrication shops that require high surface quality and the ability to process different sheet thicknesses.
Choosing the proper die design is the first part of the equation. The second is the proper adjustment of the V-opening and a series of trial bends. This is essential for consistent results in production.

Comparison of contact mechanisms between conventional fixed die shoulders and rotating roller shoulders. Roller rotation helps reduce sliding friction and surface scuffing. Diagram is not drawn to scale.
Why Does a Press Brake Leave Die Marks?
During conventional air bending, the sheet metal is supported by two shoulders of the lower V-die while the upper punch moves downward into the die opening. As the bending process progresses, the sheet slides across the die shoulders.
When contact pressure is high, or when the die shoulders contain material buildup, 버, or metal chips, this sliding motion can produce visible witness lines, scuff marks, scratches, or localized indentations.
It is essential to determine where the marks occur, prior to selecting a corrective solution.
•Two parallel marks on the outer surface near the die contact points: Review the lower die shoulders for surface condition, contact geometry and cleanliness.
•Marks on the inside bend surface: Review the upper punch nose radius for surface finish and contact conditions.
Identifying where the marks occur, helps prevent tooling changes that are unnecessary and ineffective for eliminating surface defects.
It is critical to determine the difference between surface scuffing and pressure-induced indentation.
•Scuffing and scratching are defined by sliding friction, surface roughness and/or tooling contamination, as well as surface damage. Addressing friction and contact conditions is the most appropriate course of action.
•Pressure-induced indentation: More frequently seen with bending of softer sheet metal with localized contact loads. Other contributing factors include, contact pressure and load distribution at the die shoulders.
Correct selection of a non-marking press brake die depends on correctly identifying the true mechanism of marking, rather than assuming that one die design can solve all surface defects.
How Does an Adjustable Roller V Die Reduce Marking?
Roller Shoulders Reduce Sliding at the Contact Surface
A roller-type non-marking press brake die uses a mechanism with rotating die shoulders to allow sheet metal to roll over during bending. Rolling contact minimizes sliding friction. Sliding friction occurs when sheet metal is in contact with conventional fixed die shoulders.
This contact mechanism, which avoids die shoulder witness marks, should be tried out via production material to gauge its applicability for a given situation, especially if a brushed finish is to be preserved.
Even though the rollers are free to rotate, surface defects can occur due to irregular contact of the rollers and adherence of metal particles to the roller surfaces.
This is why it is critical to conduct routine maintenance and inspection to ensure surface quality is consistent.
Adjustable Openings Cover Different Bending Setups
With an adjustable V-opening roller die, the operator can change the V-die opening by moving the left and right lower die modules.
With the tooling's adjustment range, various bending configurations can be achieved with a single lower die assembly. This may prevent the need for a complete tooling changeover.
Depending on the design of the die, the following may be used to adjust a V-opening:
•Mechanisms: These allow operators to physically move die modules to the desired position.
•Spacers: These are used to set the V-opening to the desired position, and may be calibrated.
•Motors: These allow the movement of die modules mechanically.
When choosing an adjustable roller V die, consideration has to be given to the load-bearing capacity and the adjustment's accuracy.
The following are examples of key questions that may be posed to the tooling supplier to provide clarification:
•Is the opening uniform along the working length?
•Locking Mechanism: What secures the die modules after adjustment?
•What load bearing capacity does the tooling fail at?
•Is the desired opening reproduced consistently?

Physical lower die assembly showing two parallel cylindrical roller shoulders and their end mounting components.
When Is Non-Marking Tooling Worth Considering?
A non-marking press brake die should be considered if surface defects occur at the lower die shoulder contact points.
Typical applications are:
•Brushed stainless steel enclosures to prevent die marks that can disrupt the grain finish
•Elevator decorative panels where exposed metal must meet certain cosmetic requirements
•Aluminum decorative components where contact marks and indentations can occur
•Coated sheet metal covers where tooling can cause scuffs or damage the coating
•Mirror finished sheets where marks or tooling contact can affect the integrity of the finish
For highly sensitive coatings, sample part inspection should be done with the customers requirements on lighting, viewing angles and protective film.
An adjustable V-opening is dependent on the production mix. Most parts requiring the same opening can be easier to setup and maintain with a fixed lower die. However if the workshop frequently switches between different thicknesses of sheet metal, inside bending radii and part geometries, a roller V die can be more flexible.
When evaluating potential tools, manufacturers should get representative production drawings and evaluate:
•Die setup and changeover time
•First article inspection requirements and approval
•Surface finishing and rework operations
This will provide a way to evaluate if using non-marking tools provides a measurable benefit.
Roller Dies vs. Other Surface Protection Options
There are many tooling solutions to help eliminate press brake die marks and surface damage. The best option for you depends on a few factors, including your tooling options, what surface finishes are required, and the minimum required flange length.
Here is a comparison to help provide some initial options before performing trial bends.
| Tooling Solution | Suitable Applications | Key Selection Considerations |
| Conventional fixed V-die with protective film or tape | Existing tooling is suitable, but an additional protective barrier is needed | Protective material wear, trapped particles, and potential changes in bend angle |
| Polymer inserts or polyurethane lower dies | Parts requiring a softer contact surface | Allowable bending load, 재료 호환성, and replacement frequency |
| Fixed-opening roller V-die | Production primarily uses one V-opening, and sliding friction causes visible witness marks | Roller condition, contact pressure, and flange support |
| Adjustable V-opening roller die | Multiple die openings are required while minimizing sliding contact | Adjustment range, locking mechanism, parallelism, and load rating at each setting |
| Rotary-wing or cam-action bending die | Short flanges or features near the bend line require an alternative support mechanism | Workpiece support, clearance requirements, and tooling load limitations |
Cylindrical roller-shoulder dies operate differently from rotary-wing and cam-action lower dies.
Although all three mechanisms may help reduce surface damage, their minimum flange capabilities and clearance requirements are not directly interchangeable.
For parts with short flanges, holes close to the bend line, or potential geometric interference, the tooling supplier should review the part drawings to verify compatibility.
How to Choose the Right V Opening
In conventional air bending, increasing the V-die opening generally reduces the required bending force. It also increases the naturally formed inside bend radius and changes the available flange support.
Decreasing the V-opening generally leads to a larger increase in bending force and local contact loads.
Certain requirements must be fulfilled by the chosen V-opening:
•Properties of the sheet material: The thickness of the sheet material limits the minimum possible depth of the V-opening.
•Inside radius of bend: The opening has a significant effect on the natural radius of curvature that occurs during air bending.
•Minimum length of the flange: Support must be present along the length of the bending tool.
•Load capacity of the tooling: The selected opening must be within the tooling's rated load limit.
The selection of a V-opening should not be based on a rigidly fixed ratio of the thickness of the sheet material.
Roller-type dies use multiple contact points between rollers and sheet metal during a bending cycle. Operators should use the V-opening definition and load capacity charts provided by the roller-type die manufacturer, rather than assume the die geometry is like a conventional fixed V-die.
JS 라고스 프레스 브레이크 톤수 계산기 is helpful in estimating an initial bending force for conventional air bending. The calculated value should be checked against the roller die's rated load capacity and operating specs.
After a change in V-opening, operators should also check punch penetration depth and springback compensation.
A bending program that produces the proper angle with one V-opening can not be assumed to produce the same result with another opening.
Verification of angle and trial bends are necessary before releasing an adjusted set-up for production.

Two V-opening configurations of an adjustable lower die. Changing the V-opening affects bending force, inside bend radius, and flange support. No operating dimensions are provided in the illustration.
How to Prevent Marks During Setup
Dimensional accuracy and surface quality must be evaluated together during trial bending. The following steps can be taken to create a bending setup to minimize surface defects.
1. Verify Surface Requirements Using Actual Production Material
Record production material grade, 두께, 입자 방향, condition of the coating and/or protective film, 있다면요.
Determine the side of the workpiece which will be visible after final assembly. Use the representative production material to establish the surface requirement, 있다면요.
2. Clean the Sheet Metal and Tooling
Review rollers and upper tooling punch for burrs and/or material build up.
Make sure rollers are free to rotate.
3. Measure and Secure the V-Opening
Measure the V-openings at various locations on the tooling using the manufacturer's suggested procedure.
Confirm the Die centerline alignment and parallelism prior to securing the adjustment mechanism.
All of the above adjustments must be performed with the tooling unloaded. Once the adjustment is made, according to the manufacturer's recommendations, lock the mechanism in place.
4. Inspect Both Sides after Trial Bending
Review the following after the trial bend on each side.
•Unloaded Bend Angle: Measure the final bend angle to determine spring back and compare it to the minimum bend angle.
•Bend Radius: Inspect the part to see if a bend radius has been properly applied.
•Flange Dimensions: Determine the overall length of the part to establish if the part is the correct length and to determine the length of the flanges.
•Surface Conditions: Determine the condition of the films on each side of the part.
If should marks are present, review the parameters of the bend to determine if they are correct, prior to adjusting bend parameters.
5. Reinspect After Consecutive Bending Cycles
A small, representative production run is to be performed and rollers are to be evaluated for material pickup, constrained roller rotation, or roller surface damage.
The validation process should include a workpiece to assess contact conditions along the working length.
Retain samples and tooling adjustment settings approved during the validation. Also retain the settings for bending parameters and inspection, and the tooling adjustment settings for future production.
Lubrication should be carried out in accordance with tooling manufacturer's recommendations. In particular, distinguish between lubrication of roller bearings and other tooling contact surfaces.
Transferring lubricants to sheets to be painted, 코팅, bonded or which require a controlled cleanliness should be avoided.
What to Check Before Ordering a Roller Die
When making a request for a quote (RFQ) for a non-marking press brake die, provide more information than thickness and length of the material being bent.
A detailed tooling RFQ includes the following:
•Material specs: hardness and temper, 두께, condition of surface.
•Inside bend radius: 필요한 반경, and radius tolerance.
•Minimum flange length: that portion of the material that must be supported during bending.
•Bend angle tolerance: after spring-back.
•Appearance requirements: 표식, exposed surface, 그리고 코팅.
•Existing defects: die marks (with pictures that show location and appearance).
Die marks pictures allow suppliers to evaluate if tooling is damaged and if sliding friction or contact pressure is the cause of die marks.
Verify Machine and Tooling Compatibility
Determine if an adjustable roller V die is compatible with a press brake.
Important technical specs are:
•Tooling mounting interface: Clamping system of the lower die holder and machine bed.
•Die Height: Impacts available bending distance and highest location of die in the machine.
•Machine Stroke: Travel of the ram.
•Daylight opening and clearances: Space between ram and die when the ram is in its farthest forward position.
•Rated load per unit length: The maximum force that may be applied for a given V opening.
•Minimum working length: The shortest length that may be bent and/or the minimum contact length.
•Off center loading limitations: Eccentric or uneven bending loads.
•Motorized adjustment: compatibility with electric control of positioning, and safety controls, and positioning interlocks.
When evaluating a new CNC 프레스 브레이크, these requirements should be considered together to ensure the machine and tooling operate as a compatible system.
Until the configuration for an upper punch profile or general-purpose lower die has been determined, 참고 Press Brake Punch and Die Selection Guide for assistance in identifying an appropriate surface protection solution.
Depending on the requirements of the workpiece, manufacturers can evaluate roller dies and protective inserts, or other types of support mechanisms.
Get a Tooling Recommendation for Your Parts
If there are bending marks on stainless steel, aluminum or coated sheet metal components, drawings of the parts, 재료 사양, and photos of any surface defects can be helpful in determining a tooling solution.
Defining the exposed surface, the required minimum flange length, and target inside bend radius helps in evaluating machine and tooling capabilities.
Contact JS RAGOS for a tooling evaluation and share your drawings to discuss installation requirements, V-opening selection, and trial bending procedures for your application.
Send Your Drawing for a Tooling Review
FAQs About Non-Marking Press Brake Dies
질문 1: Can a Non-Marking Die Eliminate Every Visible Mark?
아니요. A non-marking press brake die is designed to minimize surface damage, but the actual results depend on material properties, contact pressure, tooling cleanliness, and coating condition.
Surface acceptability should be verified through trial bends using actual production material and the customer's specified cosmetic inspection criteria.
질문 2: Can Roller Dies Be Used for Stainless Steel and Aluminum?
네. Roller-type non-marking dies can be evaluated for both stainless steel and aluminum bending applications.
For brushed stainless steel, attention should be given to changes in the grain pattern and surface appearance. For softer aluminum alloys, localized pressure marks and indentations require additional consideration.
The suitable material thickness, alloy temper, and surface treatment must be verified against the tooling specifications and trial bending results.
질문 3: Does a Wider V-Opening Always Give a Better Finish?
꼭 그런 건 아니에요. A wider V-opening may reduce the required bending force, but it also changes the inside bend radius and flange support conditions.
Dimensional requirements and tooling load limits must be satisfied before comparing surface finish results at different V-opening settings.
Q4: Can an Adjustable Roller Die Replace All Fixed Dies?
아니요. An adjustable roller V die can accommodate multiple bending configurations within its specified adjustment range.
그렇지만, parts requiring small inside bend radii, 짧은 플랜지, acute bend angles, or special clearance conditions may still require fixed-opening dies or dedicated tooling.